CANADA’S LEADING COST AND QUALITY PERFORMANCE PURGING SOLUTION FOR INJECTION MOLDING AND BLOW MOLDING

Extrusion

^

Step 1

Maintain processing profile for resin in the machine. (minimum temperature 135°C)
^

Step 2

Empty the screw and barrel of residual resin.
^

Step 3

Place PurgeMax® directly into hopper and follow with purging material immediately. *
^

Step 4

Maintain continuous purging until the resin appears natural and clean.
^

Step 5

The Purging process is complete, resume with standard procedures for the next job.
* With applications that require more than one PurgeMax® (refer PurgeMax® Usage Chart) , place one P PurgeMax® into the hopper and follow with a small amount of purging resin (layering) and repeat until the entire dosage has been added then charge the barrel with purging resin.

Note: A small amount of smoke may appear during purging. Although not very common, it is a normal condition.