CANADA’S LEADING COST AND QUALITY PERFORMANCE PURGING SOLUTION FOR INJECTION MOLDING AND BLOW MOLDING
BLOW MOLDING
Step 1
Maintain processing profile for resin in the machine. (minimum temperature 135°C)
Step 2
Empty the screw and barrel of residual resin.
Step 3
Place PurgeMax® directly into hopper and follow with purging material immediately. *
Step 4
The Purging process can be done by purging or injection. **
Step 5
Maintain continuous purging until resin appears natural and clean.
Step 6
The Purging process is complete, resume with standard procedures for next job.
* With applications that require more than one PurgeMax® (refer PurgeMax® Usage Chart) , place one PurgeMax into the hopper and follow with a small amount of purging resin (layering) and repeat until entire dosage has been added then charge the barrel with purging resin.
Note: A small amount of smoke may appear during purging. Although not very common, it is a normal condition.